Mechanical properties of thermoformed and direct-printed aligner materials after immersion in 37 °C water: a 14-day in vitro study

Compares mechanical properties of thermoformed and direct-printed aligner materials after 14 days in body-temperature water.

Scientific Reports

Mechanical properties of thermoformed and direct-printed aligner materials after immersion in 37 °C water: a 14-day in vitro study

Published in Scientific Reports (2026). Compares mechanical properties of thermoformed and direct-printed aligner materials after 14 days in body-temperature water.